| পরিমাণ: | |
|---|---|
17-99,17-88
| হাইড্রোলাইসিস ডিগ্রী |
বিশুদ্ধতা |
সান্দ্রতা এমপিএ |
উদ্বায়ী |
পিএইচ |
ছাই |
NaAc |
|
| 05-88 |
87.0-89.0% |
≥93.5% |
4.5-6.0 |
≤5.0% |
5-7 |
≤0.4% |
|
| 17-88 |
87.0%-89.% |
≥93.5% |
21.0-29.0 |
≤5.0% |
5-7 |
≤0.4% |
|
| 20-88 |
87.0%-89.% |
≥93.5% |
29.1-44.0 |
≤5.0% |
5-7 |
≤0.3% |
|
| 24-88 |
87.0%-89.% |
≥93.5% |
48.0-59.9 |
≤5.0% |
5-7 |
≤0.3% |
|
| 26-88 |
87.0%-89.% |
≥93.5% |
≥60.0 |
≤5.0% |
5-7 |
≤0.3% |
|
| 17-92 |
90.0-94.0% |
≥93.5% |
28.0-34.0 |
≤5.0% |
5-7 |
≤0.4% |
|
| 17-99 |
99.3-100.0% |
≥94.0% |
23.0-33.0 |
≤5.0% |
5-7 |
≤0.7% |
≤1.5% |
| 17-99L |
98.2-98.8% |
≥94.0% |
28.0-32.0 |
≤5.0% |
5-7 |
≤0.7% |
≤1.5% |
| 20-99 |
99.3-100.0% |
≥94.0% |
45.1-55.0 |
≤5.0% |
5-7 |
≤0.7% |
≤1.5% |
| 24-99 |
99.3-100.0% |
≥94.0% |
65.0-78.0 |
≤5.0% |
5-7 |
≤0.7% |
≤1.5% |
| 26-99 |
99.3-100.0% |
≥94.0% |
78.1-82 |
≤5.0% |
5-7 |
≤0.7% |
≤1.5% |
| 26-99C |
99.3-100.0% |
≥94.0% |
≥83.0 |
≤5.0% |
5-7 |
≤0.7% |
≤1.5% |
এক্সিকিউটিভ স্ট্যান্ডার্ড:Q/SXHB.3002-2013
প্যাকিং: 20/25 কেজি প্লাস্টিকের বোনা ব্যাগ বা কাগজের ব্যাগ, 750/1000 কেজি বোনা ব্যাগ
পরিবহন: আর্দ্রতা, বৃষ্টি এবং রোদ প্রতিরোধ করার জন্য একটি পরিষ্কার পরিবহণ ব্যবহার করা এবং প্যাকিং স্ক্র্যাচ বা চূর্ণ রোধ করতে আলতোভাবে চলাফেরা করা।
সংগ্রহস্থল: উপাদান ছাঁচনির্মাণ এবং deteriorating কোনো ঝুঁকি সঙ্গে খুব স্থিতিশীল. শুষ্ক অবস্থার অধীনে. আর্দ্রতা থেকে সুরক্ষিত যখন অনির্দিষ্ট.