Kwa kuwa wanywaji wa sehemu PVA ina vikundi zaidi vya acetate, na kiasi cha kikundi cha acetate ni kubwa zaidi kuliko kundi la hydroxyl, kuna kizuizi kikubwa cha steri, ili sehemu iliyoletwa kwa sehemu PVA haiwezi kuunda muundo wa kioo. It can only form loose structures with large spaces between molecules, which can absorb more air.In the process of boiling size,because the size has a certain viscosity,it provents the small bubbles from escaping from the size surface,and forms the accumulation of small bubbles,which produces greater energy,thus making the size overflow the size mixing kettle.If there still is bubble in the sizing box,a foam layer will form form on Uso wa ukubwa, ambao utaathiri uendeshaji wa mfanyakazi na pia unaathiri ubora wa ukubwa.
Njia ya kuondoa povu ni kuongeza wakala wa antifoaming kwenye sanduku la sizing au kettle ya kuchanganya. Wakala wa antifoaming kwa kweli ni sufactant na vikundi vichache vya hydrophilic, ambavyo vinaweza kupunguza mvutano wa uso wa povu na kuvunja haraka foam, kwa hivyo kupunguza mkusanyiko wa foam na kusudi la kuharibika kwa haraka.